This standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels (UTS = 1450 MPa), stainless steels (UTS = 1450 MPa), copper alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard. The purpose of this standard is to give technical and quality requirements of Zinc-Nickel plating. It doesn?t give complete in-house process instructions, these shall be given in the manufacturers detailed process instructions.
Author | ASD-STAN |
---|---|
Editor | ASD-STAN |
Document type | Draft |
Format | File |
Cancellation date | 2014-12-01 |
Edition | P1 |
ICS | 49.040 : Coatings and related processes used in aerospace industry |
Number of pages | 13 |
Cross references | 12/30263299 DC (2012-04-11), IDT |
Set | ASDPRENSET |
Year | 2013 |
Document history | ASD-STAN prEN 4826 (2013-03-31) |
Country | Belgium |
Keyword | ASD 4826;EN 4826;prEN 4826;4826 |